Silicon strontium alloy
Features
1.The best inoculation effect can be obtained in medium-sulfur and high-sulfur cupola molten iron or sulfur-enriched electric furnace molten iron.
2.Conducive to inoculation in low rare earth nodular cast iron, increase the number of graphite balls.
3.The effect of preventing white mouth is significant, the duration is long, and the number of eutectic clusters is not increased.
4.The extremely low aluminum and calcium content is easy to melt, which can significantly reduce casting defects caused by slag inclusions and shrinkage.
Supply granularity
0.1-0.5mm、 0.2-0.7mm、 1-3mm,It can process various special specifications according to user requirements。
Product packaging
25kg iron woven bag packaging plus ton bag packaging。
Quality assurance